期刊论文详细信息
Materials 卷:13
Surface Comparison of Three Different Commercial Custom-Made Titanium Meshes Produced by SLM for Dental Applications
João Paulo Tondela1  Nuno Cruz2  Javier Gil Mur2  Maria Inês Martins3  José Domingos Santos4 
[1] CIROS from the Faculty of Medicine, University of Coimbra, 3004-504 Coimbra, Portugal;
[2] Faculty of Dentistry, Universitat Internacional de Catalunya, 08017 Barcelona, Spain;
[3] Faculty of Engineering. University of Porto (FEUP), 4200-465 Porto, Portugal;
[4] REQUIMTE-LAQV, Department of Metallurgical Engineering and Materials, Faculty of Engineering. University of Porto (FEUP), 4200-465 Porto, Portugal;
关键词: biomaterial;    bone regeneration;    titanium mesh;    3D printing;    surface properties;    roughness;   
DOI  :  10.3390/ma13092177
来源: DOAJ
【 摘 要 】

The use of individualized titanium meshes has been referred to in scientific literature since 2011. There are many advantages to its use, however, the main complications are related to early or late exposures. As some aspects such as its surface properties have been pointed out to influence the soft tissue response, this study was designed to compare the surface characteristics of three commercially available individualized titanium meshes between them and according to the manufacturer’s specifications. The results from the scanning electron microscopy, energy-dispersive X-ray spectroscopy, X-ray diffraction and the contact profilometry measurements were analyzed and cross-checked. It was discovered that, the BoneEasy’s post-processing superficial treatment was more refined, as it delivers the mesh with the lowest Ra value, 0.61 ± 0.14 µm, due to the applied electropolishing. On the other hand, the Yxoss CBR® mesh from ReOss® was sandblasted, presenting an extremely rough surface with a Ra of 6.59 ± 0.76 µm.

【 授权许可】

Unknown   

  文献评价指标  