Hanford Immobilized LAW Product Acceptance: Tanks Focus Area Testing Data Package II | |
Schulz, Rebecca L. ; Lorier, Troy H. ; Peeler, David K. ; Brown, Kevin G. ; Reamer, Irene A. ; Vienna, John D. ; Jiricka, Antonin ; Jorgensen, Benaiah M. ; Smith, Donald E. | |
Pacific Northwest National Laboratory (U.S.) | |
关键词: Corrosion; Low-Activity Waste; Testing; Durability; Wastes Glass; | |
DOI : 10.2172/15001113 RP-ID : PNNL-13344 RP-ID : AC05-76RL01830 RP-ID : 15001113 |
|
美国|英语 | |
来源: UNT Digital Library | |
【 摘 要 】
This report is a continuation of the Hanford Immobilized Low Activity Waste (LAW) Product Acceptance (HLP): Initial Tanks Focus Area Testing Data Package (Vienna et al. 2000). In addition to new 5000-h product consistency test (PCT), vapor hydration test (VHT), and alteration products data, some previously reported data together with relevant background information are included for an easily accessible source of reference when comparing the response of the various glasses to different test conditions. A matrix of 55 glasses was developed and tested to identify the impact of glass composition on long-term corrosion behavior and to develop an acceptable composition region for Hanford LAW glasses. Of the 55 glasses, 45 were designed to systematically vary the glass composition, and 10 were selected because large and growing databases on their corrosion characteristics had accumulated. The targeted and measured compositions of these glasses are found in the Appendix A. All glasses were fabricated according to standard procedures and heat treated to simulate the slow cooling that will occur in a portion of the waste glass after vitrification in the planned treatment facility at Hanford.
【 预 览 】
Files | Size | Format | View |
---|---|---|---|
15001113.pdf | 2794KB | download |