期刊论文详细信息
SURFACE & COATINGS TECHNOLOGY 卷:206
Galvanic corrosion of Ni-Cu-Al composite coating and its anti-fouling property for metal pipeline in simulated geothermal water
Article
Wang, G. G.1  Zhu, L. Q.1  Liu, H. C.1  Li, W. P.1 
[1] Beihang Univ, Sch Mat Sci & Engn, Key Lab Aerosp Mat & Performance, Minist Educ, Beijing 100191, Peoples R China
关键词: Composite coating;    Galvanic corrosion;    CaCO3 fouling;    Surfaces;    Anti-fouling;   
DOI  :  10.1016/j.surfcoat.2012.02.054
来源: Elsevier
PDF
【 摘 要 】

A novel anti-fouling epoxy-silicone composite coating containing Ni-Cu-Al alloy powder for metal pipeline in geothermal water was fabricated based on the basic principles of galvanic corrosion. Fouling behaviors of the surface of composite coating in the simulated geothermal water were studied in comparison with stainless steel and epoxy-silicone resin coating. The results indicated that composite coating possessed a good anti-fouling performance. In the geothermal water, Ni2+, Cu2+ and Al3+ ions, originated from interface electrochemical corrosion, were released into bulk solution. These metal ions intensively inhibited nucleation and crystal growth rate of CaCO3 fouling on the surface of composite coating, and promoted precipitation of CaCO3 fouling in the bulk-solution, which could be easily washed away by flowing water. But for 304 stainless-steel and epoxy-silicone resin coating. CaCO3 fouling grew easily and adhered firmly to their surfaces, and influenced the transport efficiency of geothermal water for pipelines. (C) 2012 Elsevier B.V. All rights reserved.

【 授权许可】

Free   

【 预 览 】
附件列表
Files Size Format View
10_1016_j_surfcoat_2012_02_054.pdf 980KB PDF download
  文献评价指标  
  下载次数:0次 浏览次数:0次