International Journal of ChemTech Research | |
Electrochemical Behaviour of NI-TI Super Elastic Shape Memory Alloy in Artificial Saliva | |
article | |
A.Anandan1  Susai Rajendran2  J.Sathiyabama3  D.Sathiyaraj1  | |
[1] SKV Higher Secondary School;Corrosion Research Centre, Department of Chemistry, St Antony’s College of Arts and Sciences for Women;PG and Research Department of Chemistry, GTN Arts College | |
关键词: Ni-Ti Super Elastic Shape Memory alloy (SESM); Artificial saliva; Limcee-500mg; Shelcal-500 mg; Corrosion resistance; Polarization study and AC Impedance spectra; | |
DOI : 10.20902/IJCTR.2018.110205 | |
学科分类:农业科学(综合) | |
来源: Sphinx Knowledge House | |
![]() |
【 摘 要 】
The aim of present study is to investigate corrosion resistance of orthodontic wiremade of Ni-Ti Super Elastic Shape Memory alloy in artificial saliva in the presence ofLimcee-500 mg and Shelcal-500 mg has been evaluated by polarization study and ACimpedance spectra, artificial saliva taken as control. It is observed that in presence of theLimcee-500 mg the corrosion resistances of Ni-Ti SESM alloy increases. On the other hand inthe presence of the Shelcal-500 mg the corrosion resistances of Ni-Ti SESM alloy decreases.Corrosion resistance increases due to linear polarisation resistance increases and corrosioncurrent values decreases. It is suggested that people implanted with orthodontic wire made ofNi-Ti SESM alloy need not hesitate to take Limcee-500 mg but Shelcal-500 mg should avoidorally. The increase or decrease in corrosion resistance of Ni-Ti SESM alloy in presence ofthese tablets in artificial saliva is due to the ingredients present in tablets.