Journal of Applied Oral Science | |
Hydroxyapatite crystallinity does not affect the repair of critical size bone defects | |
José Mauro Granjeiro1  Gloria de Almeida Soares2  Marcio Baltazar Conz3  | |
[1] Universidade Federal Fluminense;Universidade Federal do Rio de Janeiro;Universidade do Grande Rio; | |
关键词: Hydroxyapatite; Bone grafting; Rats; Histology; Biocompatibility testing; | |
DOI : | |
来源: DOAJ |
【 摘 要 】
OBJECTIVE: The physicochemical properties of hydroxyapatite (HA) granules were observed to affect the biological behavior of graft materials. The aim of this work was to analyze the tissue response of two HA granules with different crystallinity and Ca/P ratio in vivo. MATERIAL AND METHODS: The HA granules were produced in the Biomaterials Laboratory (COPPE/UFRJ). The testing materials were HA granules presenting a Ca/P molar ratio of 1.60 and 28% crystallinity (HA-1), and a Ca/P molar ratio of 1.67 and 70% crystallinity (HA-2). Both HAs were implanted into a critical-size calvaria rat defects. RESULTS: To note, in the control group, the bone defects were filled with blood clot only. Descriptive and histomorphometric analyses after 1, 3, and 6 months postoperatively showed mild inflammatory infiltrate, mainly comprising macrophage-like and multinucleated giant cells, and an increase in the volume density of the fibrous tissues (p<0.05), which was in contrast to the similar volume density of the newly formed bone and biomaterials in relation to the control group. CONCLUSION: Thus, we concluded that HA-1 and HA-2 are biocompatible and non-degradable, and that crystallinity does not affect bone repair of critical size defects.
【 授权许可】
Unknown