[1] Center for X-ray Analytics, Empa, Swiss Federal Laboratories for Materials Science and Technology, Überlandstrasse 129, 8600 Dübendorf, Switzerland;Laboratory for Advanced Fibers, Empa, Swiss Federal Laboratories for Materials Science and Technology, Lerchenfeldstrasse 5, 9014 St. Gallen, Switzerland;Corresponding author.;Laboratory for Advanced Fibers, Empa, Swiss Federal Laboratories for Materials Science and Technology, Lerchenfeldstrasse 5, 9014 St. Gallen, Switzerland; | |
关键词: Wide-angle x-ray diffraction; Polarized attenuated total reflection Fourier Transform infrared spectroscopy; P3HB; poly(3-hydroxybutyrate); Biodegradable; Melt-spun; | |
DOI : | |
来源: DOAJ |
【 摘 要 】
This article summarizes synchrotron wide-angle x-ray diffraction (WAXD) patterns, polarized attenuated Fourier transform infrared spectroscopy (ATR-FTIR) data and differential scanning calorimetry (DSC) data of differently stress-annealed poly(3-hydroxybutyrate) (P3HB) fibers. Additionally, in-situ polarized ATR-FTIR data has been measured under tensile drawing of pre-annealed P3HB fibers under low annealing stress. Modifications to the ATR-FTIR setup and sample holders for performing measurements on P3HB fibers are explained in the experimental section. For more information see ‘Reversible mesophase in stress-annealed poly(3-hydroxybutyrate) fibers: A synchrotron x-ray and polarized ATR-FTIR study' [1].
【 授权许可】
Unknown