BioMedical Engineering OnLine | |
Examination of ceramic restoration adhesive coverage in cusp-replacement premolar using acoustic emission under fatigue testing | |
Yen-Hsiang Chang1  Jin-Jie Yu2  Chun-Li Lin2  | |
[1] Department of General Dentistry, Chang Gung Memorial Hospital, Ding-Hu Road, Kuei-Shan, Tao-Yuan 333, Taiwan | |
[2] Department of Biomedical Engineering, National Yang-Ming University, No.155, Sec.2, Linong Street, Taipei 112, Taiwan | |
关键词: CAD/CAM; Fatigue; Acoustic emission; Ceramic; Cuspal-coverage; | |
Others : 1084184 DOI : 10.1186/1475-925X-13-165 |
|
received in 2014-08-26, accepted in 2014-11-19, 发布年份 2014 | |
【 摘 要 】
Background
This study investigates CAD/CAM ceramic cusp-replacing restoration resistance with and without buccal cusp replacement under static and dynamic cyclic loads, monitored using the acoustic emission (AE) technique.
Method
The cavity was designed in a typical MODP (mesial-occlusal-distal-palatal) restoration failure shape when the palatal cusp has been lost. Two ceramic restorations [without coverage (WOC) and with (WC) buccal cuspal coverage with 2.0 mm reduction in cuspal height] were prepared to perform the fracture and fatigue tests with normal (200 N) and high (600 N) occlusal forces. The load versus AE signals in the fracture and fatigue tests were recorded to evaluate the restored tooth failure resistance.
Results
The results showed that non-significant differences in load value in the fracture test and the accumulated number of AE signals under normal occlusal force (200 N) in the fatigue test were found between with and without buccal cuspal coverage restorations. The first AE activity occurring for the WOC restoration was lower than that for the WC restoration in the fracture test. The number of AE signals increased with the cyclic load number. The accumulated number of AE signals for the WOC restoration was 187, higher than that (85) for the WC restoration under 600 N in the fatigue test.
Conclusion
The AE technique and fatigue tests employed in this study were used as an assessment tool to evaluate the resistances in large CAD/CAM ceramic restorations. Non-significant differences in the tested fracture loads and accumulated number of AE signals under normal occlusal force (200 N) between different restorations indicated that aggressive treatment (with coverage preparation) in palatal cusp-replacing ceramic premolars require more attention for preserving and protecting the remaining tooth.
【 授权许可】
2014 Chang et al.; licensee BioMed Central Ltd.
【 预 览 】
Files | Size | Format | View |
---|---|---|---|
20150113155139281.pdf | 1343KB | download | |
Figure 5. | 62KB | Image | download |
Figure 4. | 64KB | Image | download |
Figure 3. | 54KB | Image | download |
Figure 2. | 58KB | Image | download |
Figure 1. | 53KB | Image | download |
【 图 表 】
Figure 1.
Figure 2.
Figure 3.
Figure 4.
Figure 5.
【 参考文献 】
- [1]Papa J, Cain C, Messer HH: Moisture content of vital vs endodontically treated teeth. Endod Dent Traumatol 1994, 10:91-93.
- [2]Sedgley CM, Messer HH: Are endodontically treated teeth more brittle? J Endod 1992, 18:332-335.
- [3]Chang YH, Lin WH, Kuo WC, Chang CY, Lin CL: Mechanical interactions of cuspal-coverage designs and cement thickness in a cusp-replacing ceramic premolar restoration: a finite element study. Med Biol Eng Comput 2009, 47(4):367-374.
- [4]Al-Hiyasat AS, Saunders WP, Sharkey SW, Smith GM, Gilmour WH: Investigation of human enamel wear against four dental ceramics and gold. J Dent 1998, 26:487-495.
- [5]Chen HY, Hickel R, Setcos JC, Kunzelmann KH: Effects of surface finish and fatigue testing on the fracture strength of CAD-CAM and pressed-ceramic crowns. J Prosthet Dent 1999, 82:468-475.
- [6]Martin N, Jedynakiewicz NM: Clinical performance of CEREC ceramic inlays: a systematic review. Dent Mater 1999, 15:54-61.
- [7]Denissen H, Dozic A, van der Zel J, van Waas M: Marginal fit and short-term clinical performance of porcelain-veneered CICERO, CEREC, and Procera onlays. J Prosthet Dent 2000, 84:506-513.
- [8]Martin N, Jedynakiewicz NM: Interface dimensions of CEREC-2 MOD inlays. Dent Mater 2000, 6:68-74.
- [9]Lin CL, Chang YH, Liu PR: Multi-factorial analysis of a cusp-replacing adhesive premolar restoration: a finite element study. J Dent 2008, 36(3):194-203.
- [10]Fennis WMM, Kuijs RH, Kreulen CM, Verdonschot N, Creugers NHJ: Fatigue resistance of teeth restored with cuspal-coverage composite restorations. Int J Prosthodont 2004, 17:313-317.
- [11]Modelli J, Steagall L, Ishikiriama A, de Lima Navarro MF, Soares FB: Fracture strength of human teeth with cavity preparations. J Prosthet Dent 1980, 43:419-422.
- [12]Lin CL, Chang CH, Ko CC: Multifactorial analysis of an MOD restored human premolar using auto-mesh finite element approach. J Oral Rehabil 2001, 28:576-585.
- [13]Fennis WMM, Kuijs RH, Kreulen CM, Roeters FJM, Creuger NHJ, Burgersdijk RCW: A survey of cusp fractures in a population of general dental practices. Int J Prosthodont 2002, 15:559-563.
- [14]Bader JD, Martin JA, Shugars DA: Incidence rates for complete cusp fracture. Community Dent Oral Epidemiol 2001, 29(5):346-353.
- [15]Lin CL, Chang YH, Chang WJ, Cheng MH: Evaluation of a reinforced slot design for CEREC system to restore extensively compromised premolars. J Dent 2006, 34:221-229.
- [16]Kuijs RH, Fennis WMM, Kreulen CM, Roeters FJM, Burgersdijk RCW: Fracture strength of cusp replacing resin composite restorations. Am J Dent 2003, 16:13-16.
- [17]Ereifej N, Silikas N, Watts DC: Initial versus final fracture of metal-free crowns, analyzed via acoustic emission. Dent Mater 2008, 24(9):1289-1295.
- [18]Roques A, Browne M, Thompson J, Rowland C, Taylor A: Investigation of fatigue crack growth in acrylic bone cement using the acoustic emission technique. Biomaterials 2004, 25(5):769-778.
- [19]Berkovits A, Fang D: Study of fatigue crack characteristics by acoustic emissions. Eng Frac Mech 1995, 51(3):401-416.
- [20]Lin CL, Chang YH, Pai CA: Evaluation of failure risks in ceramic restorations for endodontically treated premolar with MOD preparation. Dent Mater 2011, 27(5):431-438.
- [21]Alander P, Lassila LV, Tezvergil A, Vallittu PK: Acoustic emission analysis of fiber-reinforced composite in flexural testing. Dent Mater 2004, 20(4):305-312.
- [22]Duray SJ, Menis DL, Gilbert JL, Greener EH: Laser–induced acoustic emission in particle filled dental composites. J Dent Res 1995, 74:184.
- [23]Fennis WM, Tezvergil A, Kuijs RH, Lassila LV, Kreulen CM, Creugers NH: In vitro fracture resistance of fiber reinforced cusp-replacing composite restorations. Dent Mater 2005, 21(6):565-572.
- [24]Kim KH, Okuno O: Microfracture behaviour of composite resins containing irregular-shaped fillers. J Oral Rehabil 2002, 29(12):115311-115319.
- [25]Vallittu PK: Use of woven glass fibres to reinforce a composite veneer: a fracture resistance and acoustic emission study. J Oral Rehabil 2002, 29(5):423-429.
- [26]Asaoka K: Effect of transient stress on acoustic emission behaviour during firing of dental porcelain. J Mater Sci 1992, 27:3118-3122.
- [27]Lin CL, Kuo WC, Yu JJ, Huang SF: Examination of ceramic restorative material interfacial debonding using acoustic emission and optical coherence tomography. Dent Mater 2013, 29(4):382-388.
- [28]Shiau YY, Wang JS: The effects of dental condition on hand strength and maximum bite force. Cranio 1993, 11:48-54.
- [29]Widmalm SE, Ericsson SG: Maximal bite force with centric and eccentric load. J Oral Rehabil 1982, 9:445-450.
- [30]DeLong R: Intra-oral restorative materials wear: rethinking the current approaches: how to measure wear. Dent Mater 2006, 22(8):702-711.
- [31]Ehrenberg DS, Weiner S: Changes in marginal gap size of provisional resin crowns after occlusal loading and thermal cycling. J Prosthet Dent 2000, 84(2):139-148.
- [32]DeLong R, Sakaguchi RL, Douglas WH, Pintado MR: The wear of dental amalgam in an artificial mouth: a clinical correlation. Dent Mater 1985, 1:238-242.
- [33]Sakaguchi RL, Douglas WH, DeLong R, Pintado MR: The wear of a posterior dental composite in an artificial mouth: a clinical correlation. Dent Mater 1986, 2:235-240.
- [34]Li H, Li J, Yun X, Liu X, Fok AS: Non-destructive examination of interfacial debonding using acoustic emission. Dent Mater 2011, 27(10):964-971.
- [35]Hannig C, Westphal C, Becker K, Attin T: Fracture resistance of endodontically treated maxillary premolars restored with CAD/CAM ceramic inlays. J Prosthet Dent 2005, 94:342-349.
- [36]Erickson RL, De Gee AJ, Feilzer AJ: Fatigue testing of enamel bonds with self-etch and total-etch adhesive systems. Dent Mater 2006, 22(11):981-987.
- [37]Wiskott A, Nicholls J, Belser U: Fatigue resistance of soldered joints: a methodological study. Dent Mater 1994, 10:215-220.
- [38]Romão W Jr, Miranda WG Jr, Cesar PF, Braga RR: Correlation between microleakage and cement thickness in three Class II inlay ceramic systems. Oper Dent 2004, 29(2):212-218.
- [39]Hibbeler RC: Mechanics of materials. 7th edition. New Jersey: Prentice Hall Co, Inc; 2007:125-127.
- [40]Yu JJ: Monitoring dental adhesive layer failure and clinical application under cycling load. Master ThesisNational Yang-Ming University, 2013