| Effects of 108 Days Tritium Exposure on UHMW-PE, PTFE, and Vespel(R) | |
| Clark, E.A. | |
| Savannah River Site (S.C.) | |
| 关键词: Research Programs; Tritium; Ambient Temperature; 36 Materials Science; Radiation Effects; | |
| DOI : 10.2172/810124 RP-ID : WSRC-TR-2002-00477 RP-ID : AC09-96SR18500 RP-ID : 810124 |
|
| 美国|英语 | |
| 来源: UNT Digital Library | |
PDF
|
|
【 摘 要 】
Samples of three polymers, Ultra-High Molecular Weight Polyethylene (UHMW-PE), polytetrafluoroethylene (PTFE), also known as Teflon(R), and Vespel(R) polyimide were exposed to 1 atmosphere of tritium gas at ambient temperature for 108 days. Sample mass and size measurements to calculate density, spectra-colorimetry, dynamic mechanical analysis (DMA), and Fourier-transform infrared spectroscopy (FT-IR) were employed to characterize the effects of this exposure on these samples. This technical report is the first report from this research program.