| SCRIPTA MATERIALIA | 卷:132 |
| Effect of heating rate during primary crystallization on soft magnetic properties of melt-spun Fe-B alloys | |
| Article | |
| Zang, B.1  Parsons, R.1  Onodera, K.2  Kishimoto, H.2  Kato, A.2  Liu, A. C. Y.3,4  Suzuki, K.1  | |
| [1] Monash Univ, Dept Mat Sci & Engn, Clayton, Vic 3800, Australia | |
| [2] Toyota Motor Co Ltd, Mishu Ku, Shizuoka 4101193, Japan | |
| [3] Monash Univ, Monash Ctr Electron Microscopy, Clayton, Vic 3800, Australia | |
| [4] Monash Univ, Sch Phys & Astron, Clayton, Vic 3800, Australia | |
| 关键词: Nucleation; Glass transition; Random anisotropy; Coerdvity; Grain size; | |
| DOI : 10.1016/j.scriptamat.2017.01.030 | |
| 来源: Elsevier | |
PDF
|
|
【 摘 要 】
The structural and magnetic properties of amorphous Fe-87 - yB13Cuy (y = 0 to 1.5) annealed with a range of heating rates (a) up to 150 K/s were investigated. The lowest coercivity (H-c) for Fe87B13 after crystallization shows a dramatic decrease from 174 A/m to 6.7 A/m when a is increased from 1.7 K/s to 150 K/s. The coercivity of Fe-87 - yB13Cuy annealed at 150 K/s is reduced by Cu addition and H-c = 3.0 A/m is obtained at y = 1.5. Nano structures with a grain size of 15 to 20 nm were evident in transmission electron micrographs from these rapidly annealed alloys. (C) 2017 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.