Polymers
Introducing Deep Eutectic Solvents as a Water-Free Dyeing Medium for Poly (1,4-cYclohexane Dimethylene Isosorbide Terephthalate) PICT Nanofibers
Sadam Hussain1  Mujahid Mehdi1  Zeeshan Khatri1  Lieva Van Langenhove2  Nadir Hussain3  Ick Soo Kim3  Sana Ullah3  Muzamil Khatri3 
[1] Center of Excellence in Nanotechnology and Materials, Mehran University of Engineering and Technology, Jamshoro 76060, Pakistan;Centre for Textile Science and Engineering, Department of Materials, Textiles and Chemical Engineering, Technologiepark 907, Zwijnaarde, 9052 Gent, Belgium;Nano Fusion Technology Research Group, Division of Frontier Fibers, Institute for Fiber Engineering (IFES), Interdisciplinary Cluster for Cutting Edge Research (ICCER), Shinshu University, Tokida 3-15-1, Nagano Prefecture, Ueda 386-8567, Japan;
关键词: ultrasonic energy;    dyeing;    deep eutectic solvents;    electrospinning;    disperse dye;   
DOI  :  10.3390/polym13162594
来源: DOAJ
【 摘 要 】

Water, one of the most priceless sources of life, is becoming dangerously threatened and contaminated due to population growth, industrial development, and climatic variations. The drainage of industrial, farming, and municipal sewage into drinking water sources pollutes the water. The textile processing industry is one of the major consumers of water. Herein, the idea of water-free dyeing of electrospun poly (1, 4-cyclohexane dimethylene isosorbide terephthalate) PICT nanofibers is proposed. For this, two different deep eutectic solvents (DE solvents) were introduced as an alternative to water for the dyeing of PICT nanofibers in order to develop a water-free dyeing medium. For this, C.I. disperse red 167 was used as a model dye to improve the aesthetic properties of PICT nanofibers. PICT nanofibers were dyed by conventional batch dyeing and ultrasonic dyeing methods to investigate the effect of the dyeing technique on color buildup characteristics. Dyeing conditions such as dyeing time, temperature and, dye-concentration were optimized. Morphological and chemical characterization observations revealed a smooth morphology of dyed and undyed PICT nanofibers. The ultrasonically dyed nanofibers showed higher color strength and increased tensile strength compared to conventionally dyed nanofibers. Further, the consumption of electrical and thermal energy was also calculated for both processes. The results confirmed that the ultrasonic dyeing method can save 58% on electrical energy and 25% on thermal energy as compared to conventional dyeing.