| Catalysts | |
| Impact of H2O2 on the Lactic and Formic Acid Degradation in Presence of TiO2 Rutile and Anatase Phases under UV and Visible Light | |
| Karima Sahel1  Annika Holm2  Frederic Dappozze2  Marwa Hamandi2  Chantal Guillard2  | |
| [1] Laboratoire des Eco‐Matériaux Fonctionnels et Nanostructurés, Département Génie des Matériaux, Faculté de Chimie, Université des Sciences et de la Technologie d’Oran (USTO), Oran 3100, Algeria;University of Lyon, Université Claude Bernard Lyon 1, 2 avenue Albert Einstein F-69626, Villeurbanne, France; | |
| 关键词: photocatalysis; UV; visible light; TiO2; rutile; anatase; | |
| DOI : 10.3390/catal10101131 | |
| 来源: DOAJ | |
【 摘 要 】
The degradation rates of formic acid and lactic acid in the presence and absence of H2O2 were studied, utilizing several TiO2 catalysts: PC105 (100% anatase), MPT 625 (100% rutile), and P25 (80% anatase/20% rutile), and the results were discussed with regards to the current literature. The impact of hydrogen peroxide on the photocatalytic efficiency of eleven TiO2 samples was then determined, using commercial anatase structures (PC105, PC500, UV100), commercial mixed anatase/rutile (P25 and P90), and six rutile (two commercial samples: MPT 625 and C-R160, and four home-made rutile samples were synthesized by TiCl4 hydrolysis). The effect of catalyst surface area and TiO2 phase on the degradation rate of lactic acid (LA) and the decomposition of H2O2 was studied and discussed in regard to the active species generated. The intermediate products formed in the absence and presence of H2O2 were also an important factor in the comparison. Finally, the efficiency of the degradation of LA and formic acid (FA) in the presence of rutile and H2O2 was determined under visible light, and their reactivity was compared. The intermediate products formed in the degradation of LA were identified and quantified and compared to those obtained under UV (Ultra-Violet).
【 授权许可】
Unknown