SHEAR BOND STRENGTHS BETWEEN CERAMIC CORES AND VENEERING CERAMICS OF DENTAL BI-LAYERED CERAMIC SYSTEMS AND THE SENSITIVITY TO THERMOCYCLING
关键词: Shear bond strength;    All-ceramic;    Failure mode;    Thermocycling;   
DOI  :  
来源: DOAJ
【 摘 要 】

The purpose of this study was to investigate the bond strength between various commercial ceramic core materials and veneering ceramics of dental bi-layered ceramic combinations and the effect of thermocycling. The shear bond strength of four dental bi-layered ceramic combinations (white Cercon, yellow Cercon, white Lava, yellow Lava, IPS E.max) were tested. Metal ceramic combinations were conducted as a control group. Half of each group was subjected to thermocycling. All specimens were thereafter subjected to a shear force. The initial mean shear bond strength values in MPa ± S.D were 28.02 ± 3.04 for White Cercon Base/Cercon Ceram Kiss, 27.54 ± 2.20 for Yellow Cercon Base/Cercon Ceram Kiss, 28.43 ± 2.13for White Lava Frame/Lava Ceram, 27.36 ± 2.25 for Yellow Lava Frame/Lava Ceram, 47.10 ± 3.77 for IPS E.max Press/IPS E.max Ceram and 30.11 ± 2.15 for metal ceramic control. The highest shear strength was recorded for IPS E.max Press/IPS E.max Ceram before and after thermocycling. The mean shear bond strength values of five other combinations were not significantly different (P < 0.05). Lithium-disilicate based combinations produced the highest core-veneer bonds that overwhelmed the metal ceramic combinations. Thermocycling had no effect on the core-veneer bonds. The core-veneer bonds of zirconia based combinations were not weakened by the addition of coloring pigments.

【 授权许可】

Unknown   

  文献评价指标  
  下载次数:0次 浏览次数:0次