Poisoning and regeneration of Pt-Pd/WO3-ZrO2 short paraffin isomerization catalysts
Sergio Canavese1  Zunilda Finelli1  Mariana Busto1  Viviana M. Benitez1  Carlos R. Vera1  Juan C. Yori1 
[1] ,Instituto de Investigaciones en Catálisis y PetroquímicaSanta Fe,Argentina
关键词: poisoning;    isomerization;    WO3-ZrO2;   
DOI  :  10.1590/S0100-40422010000300003
来源: SciELO
PDF
【 摘 要 】

WO3-ZrO2 catalysts promoted with Pt and Pd were tested as paraffin isomerization catalysts using n-hexane as model compound. Sulfur and amine poisoning and regeneration tests were used to assess the impact of the addition of Pt and Pd on the deactivation resistance and regenerability. Pt and PtPd catalysts were the most active for n-hexane isomerization. The low activity of the Pd catalyst was attributed to poor Pd metal properties when supported over WO3-ZrO2 and to a decrease of the number of BrQnsted acid sites. PtPd was the only catalyst capable of full regeneration after S poisoning. Amine poisoning completely supressed the isomerization activity and the original activity could only be restored by calcination and reduction.

【 授权许可】

CC BY-NC   
 All the contents of this journal, except where otherwise noted, is licensed under a Creative Commons Attribution License

【 预 览 】
附件列表
Files Size Format View
RO202103040063133ZK.pdf 312KB PDF download
  文献评价指标  
  下载次数:5次 浏览次数:1次