Microstructure Analysis of Ti-xPt Alloys and the Effect of Pt Content on the Mechanical Properties and Corrosion Behavior of Ti Alloys | |
Ho-Jun Song2  Mi-Kyung Han2  Hyeon-Gyeong Jeong2  Yong-Tai Lee1  | |
[1] Korea Institute of Materials Science, Changwon 642-831, |
|
关键词: Ti-Pt alloys; corrosion resistance; microstructure; mechanical properties; | |
DOI : 10.3390/ma7053990 | |
来源: mdpi | |
【 摘 要 】
The microstructure, mechanical properties, and corrosion behavior of binary Ti-xPt alloys containing 5, 10, 15 and 20 wt% Pt were investigated in order to develop new Ti-based dental materials possessing superior properties than those of commercially pure titanium (cp-Ti). All of the Ti-xPt (x = 5, 10, 15, 20) alloys showed hexagonal α-Ti structure with cubic Ti3Pt intermetallic phase. The mechanical properties and corrosion behavior of Ti-xPt alloys were sensitive to the Pt content. The addition of Pt contributed to hardening of cp-Ti and to improving its oxidation resistance. Electrochemical results showed that the Ti-xPt alloys exhibited superior corrosion resistance than that of cp-Ti.
【 授权许可】
CC BY
© 2014 by the authors; licensee MDPI, Basel, Switzerland
【 预 览 】
Files | Size | Format | View |
---|---|---|---|
RO202003190025697ZK.pdf | 1944KB | download |