7th International Conference on Key Engineering Materials | |
Effect of cryogenic temperatures on the failure strain and surface morphology of glass fiber | |
材料科学;工业技术 | |
Wang, Qingwei^1 ; Jian, Chen^2 ; Lida, Luo^1 ; Wei, Ning^2 | |
State Key Laboratories for Modification of Chemical Fiber and Polymer Materials, Donghua University, Shanghai | |
201620, China^1 | |
Engineering Research Center of Advanced Glasses Manufacturing Technology, MOE, Donghua University, Shanghai | |
201620, China^2 | |
关键词: Cryogenic temperatures; Failure strain; Reinforced composites; | |
Others : https://iopscience.iop.org/article/10.1088/1757-899X/201/1/012044/pdf DOI : 10.1088/1757-899X/201/1/012044 |
|
来源: IOP | |
![]() |
【 摘 要 】
Glass fiber used as reinforced composite presented excellent properties and was used widely in various environment including cryogenic temperature. The failure strain and surface morphology of glass fiber dipped in the liquid nitrogen and room temperature were measured in the study. Through the comparison of two different environment, results showed the glass fiber present better failure strains compared to those at room temperature, and there are no visible defect in the surface of glass fiber after immerged into the liquid nitrogen. The reduction of failure strain in the room temperature would owe dominantly to the relative humidity, but the temperature just exercised less influence on it.
【 预 览 】
Files | Size | Format | View |
---|---|---|---|
Effect of cryogenic temperatures on the failure strain and surface morphology of glass fiber | 305KB | ![]() |