Fabrication and characterization of micro-band boron-doped diamond electrode for an application in adenosine phosphates sensor | |
Prayikaputri, P.U.^1 ; Gunlazuardi, J.^1 ; Ivandini, T.A.^1 | |
Department of Chemistry, Faculty of Mathematics, Natural Sciences Universitas Indonesia, Kampus UI Depok, Depok | |
16424, Indonesia^1 | |
关键词: Band electrode; BDD electrodes; Boron doped diamond; Boron doped diamond electrodes; Boron-doped diamond films; Fabrication and characterizations; Oxidation peak; Silicon rubbers; | |
Others : https://iopscience.iop.org/article/10.1088/1757-899X/188/1/012035/pdf DOI : 10.1088/1757-899X/188/1/012035 |
|
来源: IOP | |
![]() |
【 摘 要 】
Micro-band electrode was successfully fabricated by lamination method through sealing a piece of boron-doped diamond film inside a sandwich of two insulating plates, namely Teflon and silicon rubber as the gaskets. Characterization was performed using Raman and XPS spectra of the BDD film, while the fabricated micro-band was characterized by analyzing its SEM image. The electrode was examined for cyclic voltammetry of adenosine triphosphate solution, where an oxidation peak at +0.9 V vs. Ag/AgCl can be observed. The influence of scan rate and pH was also studied, in which pH 2 was selected as the optimum pH. The diffusion coefficient of 0.1 mM ATP at micro-band electrode was 3.84 x 10-8m2/s, while the effective surface of the micro-band BDD electrode was 8.72 x 10-14m2.