会议论文详细信息
4th International Conference on Civil and Environmental Engineering for Sustainability
Microbial Activity in Peat Soil Treated With Ordinary Portland Cement (OPC) and Coal Ashes
地球科学;生态环境科学;经济学
Rahman, J.A.^1 ; Mohamed, R.M.S.R.^1 ; Al-Gheethi, A.A.^1
Department of Water and Environmental Engineering, Faculty of Civil and Environmental Engineering, Universiti Tun Hussein Onn Malaysia, Parit Raja, Batu Pahat, Johor
86400, Malaysia^1
关键词: Enzymatic activities;    High moisture contents;    Microbial activities;    Ordinary Portland cement;    Solidification process;    Strength development;    Strength increments;    Water-to-binder ratio;   
Others  :  https://iopscience.iop.org/article/10.1088/1755-1315/140/1/012087/pdf
DOI  :  10.1088/1755-1315/140/1/012087
学科分类:环境科学(综合)
来源: IOP
PDF
【 摘 要 】
Peat soil is a cumulative of decayed plant fragment which developed as a result of microbial activity. The microbes degrade the organic matter in the peat soils by the production of hydrolysis enzyme. The least decomposed peat, known as fibric peat has big particles and retain lots of water. This made peat having high moisture content, up to 1500 %. The most decomposed peat known as sapric peat having fines particles and less void ratio. The present study aimed to understand the effects of solidification process on the bacterial growth and cellulase (CMCase) enzyme activity. Two types of mixing were designed for fibric, hemic and sapric peats; (i) Ordinary Portland cement (OPC) at an equal amount of dry peat, with 25 % of fly ash (FA) and total of coarse particle, a combination of bottom ash and fibre of 22 - 34 %, (ii) fibric peat was using water-to-binder ratio (w/b) = 1, 50% OPC, 25 % bottom ash (BA) and 25 % FA. For hemic and sapric peat, w/b=3 with 50 % OPC and 50 % BA were used. All samples were prepared triplicates, and were cured for 7, 14, 28 and 56 days in a closed container at room temperature. The results revealed that the first mix design giving a continuous strength development. However, the second mix design shows a decreased in strength pattern after day 28. The influence of the environment factors such as alkaline pH, reduction of the water content and peat temperature has no significant on the reduction amount of native microbes in the peat. The microbes survived in the solidified peat but the amount of microbes were found reduced for all types of mixing Fibric Mixed 1 (FM1), Hemic Mixed 1(HM1) and Sapric Mixed 1 (SM1) were having good strength increment for about 330 - 1427 % with enzymatic activity recorded even after D56. Nevertheless, with increase in the strength development through curing days, the enzymatic activities were reduced. For the time being, it can be concluded that the microbes have the ability to adapt with new environment. The reactivity of the microbes relates with the strength of solidified peat.
【 预 览 】